Anyone have any advice for better tips that make it easier to see where the actual cut will be? I have the A-81 torch. Maybe some drag tips ? Tell me what you use and what works for you
Anyone have any advice for better tips that make it easier to see where the actual cut will be? I have the A-81 torch. Maybe some drag tips ? Tell me what you use and what works for you
Get a roller guide or drag tips. For straight cuts I use an aluminum straight edge and drag the roller or tip against it... just allow for the distance between the straight edge and where the actual cut will be. Once you have the measurement you'll use that same offset every time. For short cuts and square tubing I use a speed square.
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
I use PRACTICE. Nothing substitutes for it.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
Pretty much, unless it is a long cut that I need precisely. But a lot of it transfers from my torch skills...
http://www.youtube.com/watch?v=ZcNqc2IzNrk&feature=plcp
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw