Haven't upgraded my MIG to an Everlast yet, we'll see how this winter goes, but in the meantime, my little handler 125 Hobart needs some doctoring. The cable sheath slipped down and I inadvertently arced the liner, causing the argon hose to melt. Are there any specific requirements of this hose to handle the gas, or can I pick up some (looks like 1/8 or 3/16) clear tube from Ace? Liner may be salvageable, not sure, but I may be able to just cut the last 3" off of it for now if the strike spot is an issue. Tight budget and whatnot.
Trip Bauer
Former USN HT
Everlast 200DX New Model
Hobart Handler 125 MIG
Van Norman #12
Atlas 12" engine lathe
'98 RoadKing - 84 Ironhead - 59 Ironhead