Share
Results 1 to 10 of 10

Thread: 200dx frequency effect on DC welding

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default 200dx frequency effect on DC welding

    I have a 200DX and trying out DC welding on steel and I have noticed not much effect when playing with the frequency. Sorry for my total noobilicious. What setting can be set for DC tig welding besides AMP?

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by vicrc View Post
    I have a 200DX and trying out DC welding on steel and I have noticed not much effect when playing with the frequency. Sorry for my total noobilicious. What setting can be set for DC tig welding besides AMP?
    As you have noticed, Frequency is only for AC, so is Balance (yellow knobs=AC) Arc Force is mainly a stick welding function. All the rest will have function, some different depending on mode. For steel DC welding the big one is of course Amps, followed by the pulser (blue knobs) The green knobs cover your gas settings, and downslope which is nice when using a torch switch but not needed with a pedal, as you will control upslope, downslope and slow pulsing with that.
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    Thanks Ram, great overall info on the knobs. I did try pulse with DC and could not find a good setting so ended up turning that feature off. I really don't understand the 3 pulse knob settings.

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by vicrc View Post
    Thanks Ram, great overall info on the knobs. I did try pulse with DC and could not find a good setting so ended up turning that feature off. I really don't understand the 3 pulse knob settings.
    Pulse is really an advanced feature. I wouldn't advise using it until you have more experience TIG welding. There are a few places where it can really help, but for most jobs you don't need it, especially on DC.
    Long arc, short arc, heliarc and in-the-dark!

  5. #5

    Default

    For noob pulse use. Set the pulse amps and pulse ratio at 50% and hertz at lowest setting on "low".

  6. Default

    Quote Originally Posted by performance View Post
    For noob pulse use. Set the pulse amps and pulse ratio at 50% and hertz at lowest setting on "low".
    Thanks Mark , I will try that

Similar Threads

  1. High Frequency Ground on back of 200DX
    By Shaggy in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 02-23-2014, 09:57 AM
  2. Tim has another TIG welding video featuring the PowerTIG 200DX
    By Mr120 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 22
    Last Post: 06-15-2013, 03:22 PM
  3. Effect of Gas on the Arc
    By Cippee in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 02-14-2012, 03:20 AM
  4. Effect of AC Balance control on aluminum
    By performance in forum Welding articles from Professionals (knowledge database)
    Replies: 4
    Last Post: 09-07-2011, 01:56 AM
  5. 200dx Stick Welding Questions
    By SeanMurphy265 in forum Stick Welding (SMAW)
    Replies: 5
    Last Post: 05-03-2011, 11:17 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •