Thought i would try and rig up an argon dryer will waiting on the new machine to arrive, had several different options, Some clear water filter housing's that would hold about 3/4 of a litre of desiccant thought that might a little to much. I found a milton air filter that i have had for a while and i think it will hold enough desiccant to do the job. It had an automatic drain valve in the bottom and already had a sintered bronze filter. I removed the drain and installed a shorty schrader valve in the bottom of the valve. I do not see any reason why it would not work it will hold about 6.61 cu inches of desiccant which is a little less than 1/2 a cup.
Click image for larger version. 

Name:	Argon filter 1.jpg 
Views:	926 
Size:	141.2 KB 
ID:	8574Click image for larger version. 

Name:	Argon filter 2.jpg 
Views:	689 
Size:	135.4 KB 
ID:	8575