I would just hear the area up with a torch and try to pull it out with vise grips. Heating on that end shouldn't have any impact on the rest of the crankshaft. If you concentrate the head on the outer hub rather than the shaft, it will likely be a little better.
				
			 
			
		 
			
			
			
				