Originally Posted by
Martine
I've been trying for ages to get some Lincoln rods, but here in the UK, generally, you can get any rod so long as it's a 6013. Almost every time, I've had to justify why I want a 6010 and why I don't want an "alternative" 6013 instead.
This sounds odd, as though you are trying to convince a salesman at a store to sell you the electrodes that you want. Is that the case? I searched online and sure enough, UK online suppliers sell 6013- if they bother to describe the electrode at all, that is, beyond "mild steel". Glad you were able to find some, eventually!
DaveO
Oxweld oxy acet gear
IMIG 200
PowerTIG 210 EXT... Amazing!