I never knew that; many thanks. That helps explain a great deal. Sp can you whip and pause with a 6010 on an inverter the same way you can with a transformer-rectifier?
No, they do not behave the same. I noticed this right off with 6011 on an inverter. 7018 was about the same, but the 6011 was not like a transformer or engine driven welder at all. It's almost backwards in the way arc force and arc length work. Took a little practice to get used to it. I'm sure you will pick it up in no time. I would use the same family of machine you are going to test on, inverter, transformer, or engine driven. Otherwise the differences might be a problem. My favorite used to be engine driven, but now I'm really liking the inverter.
Long arc, short arc, heliarc and in-the-dark!