Well hello there community!

My name is Donald T. From North Las Vegas.
I just recently purchase a pp256, as I have been doing quite a bit of research of these machines. Having previously owned a miller cst 280 (just sold it on ebay to fund my new machine). The miller was a great machine, only lacking in the ability to do ac. but for the price it went for on ebay, 12xx. for just a few more hundred, I got a plasma cutter and the option to weld in ac. I also bought the machine of ebay.. at around the 16th of november. took longer than expected. blame ups for that.
In any case, im in the construction Industry as an Ironworker, crane Op, structural welder. I love fabricating stuff..