I received my 225LX on 2/23/12 with a WP9 torch option, by April the rubber insulation around the flexneck had cracked and shocked the crap out of me. (I SHOULD HAVE CALLED IT IN RIGHT AWAY) I took a piece of bike tube and wrapped it around the cracked rubber and used electrical tape to seal it up. I didn't use the welder at all until about 2 weeks ago. I fired it up to do a few small aluminum parts. Today the entire neck snapped off the handle when I tried to adjust the angle of the torch head, due to brittle rubber and a poor design. The flex neck itself isn't even brazed to the copper in the handle. The only thing keeping the flexible copper wound wire attached to the copper electrical lug inside the handle is the molded rubber, which was partially melted down into the area between the wound copper flex neck and the electrical lug in the handle.(explains why the neck always got so damn hot even at low amperage) Which failed after very limited use. I am really not happy with the quality of this torch! Will everlast warranty my torch? Has anyone else had this issue? Has everlast come up with a new design on the torch????

I think I'll call in and see what Everlast is willing to do.