Thread: can't get machine to work on aluminum at home

Threaded View

Previous Post Previous Post   Next Post Next Post
  1. Default can't get machine to work on aluminum at home

    I can't seem to get this 185 to work on aluminum at home. Machine works at auto repair garage fine. Using On same circuit at home as my Dynasty which worked fine. Same extension cord I used on Dynasty. Using a 220v Dryer circuit. Tried everlast pedal/switch, everlast torch with regular lens/gas lens . Using 100% argon , tried the meter at 5,10,15

    The arc is all over the place, won't puddle. Nothing do do with cleaning material or balance /freq

    Pictures attached.
    Click image for larger version. 

Name:	IMG_1008.jpg 
Views:	445 
Size:	75.7 KB 
ID:	8819Click image for larger version. 

Name:	IMG_1009.jpg 
Views:	419 
Size:	130.7 KB 
ID:	8820
    Last edited by tictac; 12-14-2012 at 01:29 AM.

Similar Threads

  1. Replies: 1
    Last Post: 04-03-2013, 10:28 AM
  2. First aluminum welds- nothing to write home about
    By DaveO in forum TIG Welding (GTAW/GTAW-P)
    Replies: 13
    Last Post: 01-28-2013, 11:14 AM
  3. Selling I-mig 205 plus aluminum spool gun for machine
    By Rodsmachineshop in forum Buy, Sale or Trade
    Replies: 5
    Last Post: 01-18-2013, 07:16 PM
  4. Amazing Aluminum Tig Work !!
    By TD2593 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 12-24-2011, 06:51 AM
  5. welding/ machine work I know there is a better way.
    By ScratchStart in forum Heavy Equipment and Commercial Projects
    Replies: 8
    Last Post: 04-26-2011, 02:19 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •