I was recently fighting similar things on my machine. Thanks to this forum you really helped me narrow it down to a gas delivery issue. Thought maybe I had contaminated gas, or a hole in my line...turns out it was a super simple fix, that I wished didn't take me 4 days to figure out! Don't be like me! https://youtu.be/DqR_N_5xm68