  1. Default Wsd-60p

    My torch is a wsd-60p but it is on a super cut 50p so does my consumables have to be for a 50a or will the 60a consumables work

  2. #2

    Default

    Quote Originally Posted by 1960plumber View Post
    My torch is a wsd-60p but it is on a super cut 50p so does my consumables have to be for a 50a or will the 60a consumables work
    The ones for the 60 will work.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    zoama, Thanks