I brought my Imig 200 to work for my friend. All galvanized schedule 40 pipe 4" and 6", these are going to Texas just a few miles from the Mexico border. They will be going around well heads and barbed wire will be added to keep cows away from the well heads. I believe it's safe to call this over kill! I let some of the other welders try out my Imig 200, and they were all impressed. It's hard for some to believe a welder this small can put out this kind of heat! I believe their 220 outlet is on a 50 amp breaker.







I welded these L's all day long today with my Imig 200.


These are corner braces for the fence.