Had some time to play with my the new 2013-250EX lots to learn over old Hobart 400 pound transformer type welder has done me well for 36 years. Made new panel note drawing to the 2013-250EX I got if someone need PDF file PM me and I will send it to you.
Problem I have and would change on the 2013- 250EX the 220volt for the water cooler should be hooked up to the main switch to turn the 220 volt pump on when the welder is turned on. You turn off welder the pumps is still running you turn the pump off it is a problem for me the old weld turned off the pump turned off welder on pump on I will say no more.
Change number two put LED lights on or beside the switches to tell you ON or OFF or MOD it is in. I know the new 255EXT will tell you what MOD you are in but not available yet or I would have bought one.
Change number three the tig gun quick disconnect should be at 2 O’clock not at 9 O’clock that is the pin locking mechanism the hose to the water cooler pointing at 2 O’clock and has a sharp turn to get to the cooler so I change mine to have the hose at 9 O’clock down see Pics.
Change number four none love the machine.
Is this normal for the HF to keep jumping inside the torch/pedal control plug?

Click image for larger version. 

Name:	EVERLAST 2013-250EX PANEL NOTES Ref..jpg 
Views:	1003 
Size:	127.3 KB 
ID:	9643

Click image for larger version. 

Name:	250EX TESTING  ON ALUM .125.jpg 
Views:	786 
Size:	145.4 KB 
ID:	9638Click image for larger version. 

Name:	Change from 9 O'clock to 2 connection.jpg 
Views:	971 
Size:	134.4 KB 
ID:	9639Click image for larger version. 

Name:	Control Plug.jpg 
Views:	880 
Size:	136.1 KB 
ID:	9640Click image for larger version. 

Name:	Hose 2 O'clock.jpg 
Views:	832 
Size:	136.4 KB 
ID:	9641Click image for larger version. 

Name:	Hose 6  O'clock.jpg 
Views:	733 
Size:	138.2 KB 
ID:	9642