I was taking a 3F test the other day on pickled and oiled 14 gauge steel and after welding the fist side of the fillet the other side got tons of mill-scale. I've tried cleaning, brushing, cooling, everything....the test turned out good. But I feel defeated that the other side is not as nice looking. I got thinking....anyone ever use brazing flux to cure this sort of thing? Thanks - RJ