Share
Results 1 to 20 of 23

Thread: NEW 2013 EVERLAST PowerITig 200T DC DIGITAL PULSE TIG WELDER LOW 2AMP START !

Threaded View

performance NEW 2013 EVERLAST PowerITig... 03-09-2013, 04:07 AM
Rambozo Great looking little DC... 03-09-2013, 04:43 AM
Oleg Rambozo dual voltage will... 03-09-2013, 04:57 AM
performance I don't think we are dropping... 03-09-2013, 05:05 AM
DVA ~22 lb welder, looks like a... 03-09-2013, 09:06 PM
SeanMurphy265 When will these be available? 03-29-2013, 07:40 PM
Oleg in stock ! 03-29-2013, 07:49 PM
DVA What is the price? 03-30-2013, 01:46 AM
annerajb Any update on the 110v 220v ... 07-30-2013, 02:46 AM
DaveO Amazon.com is showing the... 07-30-2013, 01:54 PM
leonb Agree, this is great! 11-17-2015, 08:00 PM
fla2smoker Does the latest model of the... 04-12-2016, 08:15 PM
Previous Post Previous Post   Next Post Next Post
  1. #1

    Default NEW 2013 EVERLAST PowerITig 200T DC DIGITAL PULSE TIG WELDER LOW 2AMP START !

    One final announcement that we have to post up about the 2013 models...Another digital unit.

    One of the best niche units we have in our stable is the i-TIG 200. It's found a big following by guns smiths and other specialty manufacturers. It's a reliable, hard working unit with a LOT of capability.

    So we have considered what we can do to make a better product and improve performance and features. So we have developed a completely new I tig 200, which will fall into the digital lineup of welders that we have. It'll have similar features as the 255 EXT but as the i-tigs are DC only, it too will be DC only.

    ONE very special thing it will have is the ability to fire off at an incredible 2 amps. We've studied the market and found that there is a need for this extremely low ignition point for guys that have molds and similar products to repair. It's been a constant request, so we've added this major capability to the unit.

    Here are some comparative specs next to the current i-tig...

    Model Power-ITIG 200 Power-ITIG 200T
    Input Voltage 110/220V 50/60 Hz 220 V 50/60 Hz
    Rated Output 200 A 200 A
    OCV 60-80V 60-80 V
    Duty cycle 35%@200 amps 35% @ 200 amps
    Welding range 5-200A TIG 5-160A Stick 2-200 A TIG 2-160A Stick
    Arc Force 0-10 1-100
    Pulse amps 5-95% 2-200 amps
    Start Amps 15 A fixed 2-150 A
    End Amps 15 A fixed 2-150 A
    Up/Down Slope time 0-5 Seconds 0-25 Seconds
    Pre Flow Time 0-5 Seconds 0-5 Seconds
    Post Flow Time 0-5 Seconds 0-25 seconds
    2t/4t yes yes
    Hot Start arc amp (stick) No welding amps + 1-100%
    Hot start arc time No .1-1.5 Seconds
    Inverter Frequency 27khz 50 khz
    Anti stick function no yes
    memory no 0-9
    weight 16 kg 9.8 kg
    dimensions 425x195x310 mm same
    Protection class IP21s IP21s

    Click image for larger version. 

Name:	CaptureI200T.jpg 
Views:	1081 
Size:	16.5 KB 
ID:	9719
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	digital itig 200.jpg 
Views:	902 
Size:	132.3 KB 
ID:	9718  
    Last edited by performance; 03-09-2013 at 04:13 AM.

Similar Threads

  1. new 2013 I-tig 200T
    By redstopgreen in forum Customer Testimonials
    Replies: 1
    Last Post: 01-16-2014, 05:26 PM
  2. NEW 2013 EVERLAST PowerTig 255 EXT AC/DC DIGITAL TIG WELDER
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 256
    Last Post: 12-13-2013, 09:48 PM
  3. NEW 2013 Everlast PowerMIG 210 and 200 MIG / TIG DIGITAL WELDER
    By Oleg in forum Everlast Announcements, Contests and Promotions
    Replies: 14
    Last Post: 02-10-2013, 01:13 AM
  4. NEW 2013 EVERLAST PowerTIG 185 ACDC TIG / STICK WELDER
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 23
    Last Post: 12-24-2012, 12:43 AM
  5. NEW 2013 Everlast PowerMTS 200 MIG / DC TIG/ STICK WELDER
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 0
    Last Post: 11-22-2012, 02:20 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •