  1. Default having some problems with my PM205

    For the most part I am happy with my machine, but I am having a couple of issues. For one, the foot pedal control does not work as it is supposed to. The only way to get any kind of control is to use the machine it the 4T mode, and set the amperage on the panel. When I try to use 2T and the foot control, it acts very much like an abrupt on-off switch, and adjusting the dial on the foot control to change amperage seems to have little to no effect. I am not sure if the problem is in the foot control or the machine, as far as amperage adjustment goes, but it does not work like it is supposed to. Overall the foot pedal is a POS, since the rack gear slides off the pinion gear on the rheostat constantly. I am going to have to modify it to work correctly, which kind of sucks, since it is brand new.

    My regulator is also leaking on the high pressure side, which I noticed after quickly going through a bottle of argon.

    Aside from these two things I am happy with the machine, I just wish the thing worked like it is supposed to.

  2. #2
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Default

    Sounds like the rack and pinion on your foot pedal is off track. Usualy an easy fix, there are some other posts on this forum about that, I think on the Tig forum, or give Mike a call, he's problaby watching NASCAR right now anyway. I sure he'd be happy to help.
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

  3. #3

    Default

    Thanks Ray for your input on the pedal. Olympics now

    Jason, email me a phone number through the forum and I will give you a call. We will see what's up. I will email you my number as well.

    We have PMs off right now until we upgrade the forum. So use the email feature.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. Default

    Thanks, email sent!

  5. Default

    I have been trying to reach you guys all morning but have not got through.

  6. #6

    Default

    Quote Originally Posted by racinjason44 View Post
    I have been trying to reach you guys all morning but have not got through.
    Your message said give a call in the evening. So I thought you preferred a call at night. I just re-read it. You sent it last night. It was 9PM
    Sunday my time when you sent it, I was probably asleep.

    Will call you in 10-20 minutes.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7

    Default

    I have a friend with a pan break going to make and see if i can make a few guide and rheostat end shaft supports that just builts under the hole allready in the pedal unit so there is no drilling . The pedal assy has good brand switchs and is made good but everything new has little up dates to make it better. I love how well the 250 ex i got welds makes such nice welds and great when i have to weld oxidized pontoon boats . make my econo tig look like crap .lol just remeber all the best stuff comes from japan and china , think of that when your watching Nascar on your china made big screen tv .

  8. #8

    Default

    If you go to ace hardware they have some cool round nylon bushings that work great to keep the shaft straight while pushing down on the pedal there cheap like 20 cent each . I made a bracket out of a piece of sheet metal also to give the long shaft on the rheostat some support i used a small nylon bushing so the shaft wasnt metal to metal . If i can figure out how to do pictures on the site i can post a picture

  9. Default

    I talked to Mike for quite a bit Friday, very helpful guy. Anyways, I am still having issues with my welder, I know my foot pedal is not working as it should be, it reads extremely erratic on the multimeter. I haven't been able to reach someone in tech support today, if you guys could give me a call anytime today at 541 404 3776 that would be great, thanks!

  10. #10

    Default

    Quote Originally Posted by racinjason44 View Post
    I talked to Mike for quite a bit Friday, very helpful guy. Anyways, I am still having issues with my welder, I know my foot pedal is not working as it should be, it reads extremely erratic on the multimeter. I haven't been able to reach someone in tech support today, if you guys could give me a call anytime today at 541 404 3776 that would be great, thanks!
    Jason, I would have called earlier today, but the voicemail you left was all chopped up and you only said your number once.


    I got 541-40 buzz buzz buzz 76. Will call you now.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. 3/8th Aluminum with my PM205
    By www in forum TIG Welding (GTAW/GTAW-P)
    Replies: 30
    Last Post: 03-29-2011, 05:37 AM
  2. 30 amp breaker for PM205
    By www in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 12
    Last Post: 04-27-2010, 05:57 PM
  3. Just set up my new PM205
    By xen808 in forum Customer Testimonials
    Replies: 1
    Last Post: 03-17-2010, 08:55 PM
  4. PM205 L10-50R Plug Wiring
    By jas329 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 01-13-2010, 06:20 AM
  5. I got my new PM205
    By nooch8it in forum Customer Testimonials
    Replies: 5
    Last Post: 12-09-2009, 06:04 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •