						thanks for the help guys! I was able to build a couple catch cans for my truck that i just finished an ls1 swap in. It amazing how much better and smoother it welds with the correct gas.. haha..
Also what do you guys think about using green tungeston on aluminum? I have been using red and it works well, but my uncle who works at air gas, told me his customers like the green better. thoughts??
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
Green is only for use on transformer welders with aluminum. In ac.
Its not recommended for inverter machines. ive found lanthanated the best for aluminum on my 225 lx eith the gold or blue band.
Sent from my SGH-T889 using Tapatalk 2
Everlast PowerTIG 225LX
Everlast Power IMIG 200
							
						
					
					
						kool thanks for the advice guys! Ill be sticking with red.
Mike R.
Email: admineverlast@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x203
M-F 12 - 7PM PST
FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.
On my 225LX I use red thoriated for steel and use blue 2% lanthanated for aluminum. These have given me the best results.
Sent from my SGH-T889 using Tapatalk 2
Everlast PowerTIG 225LX
Everlast Power IMIG 200
Mike R.
Email: admineverlast@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x203
M-F 12 - 7PM PST
FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.
							
						
					
					
						What about the new all purpose Purple ones.
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
2% Thoriated and 1.5%/2% lanthanated are best, I moved to lathanated. The grey and whites, are not bad on aluminum, but not best.
Almost said the colors, but that would look like a welder ad not in our favor.
Mike R.
Email: admineverlast@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x203
M-F 12 - 7PM PST
FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.
I have been using 1.5% lanthanated for all my tig needs and have not had any problems with it even at 200A on aluminum.
Jason
Everlast 255EXT - Perfection
Everlast PowerPro 256 - UPS Demolished
Everlast MTS200s
12 Ton Shop Press
DeWalt Hand Tools/ChopSaw
i use rubbing alchol to clean my material ,mostly aluminum and i have had bad argon gas that i have had to exchange.i also make catch cans and intercooler tanks .
250 ex
205 mig
milwaukee grinder
140e mig
Never use brake cleaner. One of the ingredients when heated in the presence of argon creates phosgene gas and will kill you with as little as one drop.
Read this
http://www.brewracingframes.com/id75.htm
Sent from my Nexus 7 using Tapatalk 2
Don
MTS 200 workhorse
PowerTig 250EX <---sweet
80 amp HF inverter arc welder
Lincoln Buzzbox
Rotobrute AC-35 Mag Drill
Milwaukee mag drill
HF Heavy Duty 16 Speed Bench Drill Press (Custom made Adjustable Height stand)
I gotta find more junk to sell on EBaY ... Must Buy a Plasma Cutter and a Mig Welder
Fullerton, Ca
USA
							
						
					
					
						Yes I know about brake cleaners. Although I am not sure where to but chlorinated brake cleaner any more. None of the parts store around me sell it. I prefer the non chlorinated stuff better anyways. I always use acetone but wanted to try something else just to eliminate possibilities. thus far it has been working great! Been making lots of catch cans, welding bungs and fitting into inductions, etc. I work at a performance shop so fabrication is a typical thing for me, but using tig welders I am new to.
Careful, it is NOT just brake cleaners. It is any solvent that uses CFC as a propellent.
Everlast PowerPro 256 (2013)
Northern Hybrid 200 & ST80i
HF 90Amp FluxCore (Don't laugh, it is what got me started)
Lotos LT5000D Plasma
HF 4x6 Horizontal Bandsaw
Rikon 18" Bandsaw w/VFD
Delta 14" Drill Press
Robland NLX31 Euro Combo WW