Been a while so I decided I would post some quick projects I have been working on with my 200DX. Everything I do is pretty much automotive related.
Schedule 40 304SS Piping for a turbo manifold. Beveled edge and backpurged and the inside looks just like the outside as seen here with full penetration.
Schedule 40 304SS Collector for previous manifold.
Aluminium Icebox for Turbo Car
Catch Can
![]()