I was welding last night(aluminum) and stopped to reposition my work(thin work with little amps). Went to start back welding and only has HF start. I even tried striking the arc directly to the ground glamp but no luck. Tried a diff foot pedal and the factory hand trigger setup. Few notes, reads around -032 amps and the display will not change no matter what knob I turn. When I try to strike the arc it basicly flashes to 000 on the display.
This couldnt have happened at a worst time, have a customer flying in this saturday and I have just a little welding left to finish for him
.
Any ideas?? Anyone at everlast feel free to call me at 434-470-2700 if needed or you have some ideas please