After neglecting my Supre Cut 50P for a couple of weeks go to use it, light off once, cut for 1/4" arc then it quit.
Shows power, no error light 62lbs dry air. Tried new consumables, nothing.
Also the regulator has taken to making a hissing sound.
Of course I need it this weekend to pick up a couple of bucks.
Has not been my month on anything involves electricity.
Suggestions please.