If I have a duty cycle of 35% at 160 amperage with a 1/8 Rod how do I calculate my duty cycle at 125 average With a 1/8 rod?
If I have a duty cycle of 35% at 160 amperage with a 1/8 Rod how do I calculate my duty cycle at 125 average With a 1/8 rod?
From the online manualhttp://www.everlastgenerators.com/do...ST-160-200.pdf
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
Figure about 5 minutes on and 5 minutes off. Normally you need more filler or ER, so the delay to get another rod might work where you are working 100% though yours power at 50-60% duty cycle wise.