  1. Question Split 3/32" filler rod into two ~0.046" rods?

    I have some excess 3/32 aluminum and steel filler rods and wanted to ask you gurus if any 'ol' shop trick exists that makes it easy to split a 3/32" thick filler rod in half so you get 2 ~0.046" thick rods? (Thereby, resulting in 2 thinner filler rods)?

    The filler rods that are thinner than 1/16 make it much easier for me to weld on thin walled tube, so just trying to make use of what I have..
    Last edited by Welderooni; 07-27-2013 at 10:46 AM.

Similar Threads

  1. Understanding "Arc Force" and how to set for different rods
    By aland in forum Stick Welding (SMAW)
    Replies: 20
    Last Post: 01-27-2018, 04:00 AM
  2. Replies: 11
    Last Post: 10-30-2012, 06:43 PM
  3. Alcotec 1/8" x 36" R4043 Filler Rod 10 Pound Boxes
    By cbmkr in forum Buy, Sale or Trade
    Replies: 0
    Last Post: 10-29-2012, 06:00 PM
  4. Replies: 2
    Last Post: 08-27-2012, 03:21 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •