Share
Results 1 to 11 of 11

Thread: tig welding noob. i need help!!!

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default tig welding noob. i need help!!!

    hey all. ive been welding fr a while but am extremely new to tig. i just got a everlast 200dx with pure argon. having alot of trouble using filler material. im using 1/16 ceriated and usng 3/32 4043 filler rod. i think the filler material is to big? welding on 1/16 peice of aluminum with 55-65 amps. some times the weld turns out good, others its absoluely discusting. im keeping the tungsten close to the work peice. seems pretty consistent as well as the travel speed. ive watched like 1000 videos on this but im just not getting it. would really appreciate the help from a experienced welder. thanks guys.
    also i know its probably from the aluminum getting hot but seems like im like blowing through it sometimes. or maybe i am raisng the tungsten up higher wih out realizing it.
    Last edited by steve1989; 07-30-2013 at 06:18 PM.

  2. #2

    Default

    START with steel. Get that down, then stainless, THEN aluminum.

  3. #3
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Welcome, Steve! Congrats on the new machine, you chose a good one. What kind of welding have you done in the past? O/A translates readily to TIG because of the coordination between hands, one for torch one for filler. Mark's idea about starting with steel has a lot of merit- you can turn off or disregard all the AC settings and concentrate on technique. You might try simply running a TIG bead with no filler at first, then add filler later.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  4. Default

    thanks guys for the great info. im going try and experiment with steel next then. can you recommend a good tungsten? i have some 3/32 purple but not hereing great things about them. also whats the best filler material for steel and best one for stainless?

  5. #5
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Not sure if you've seen these videos (among your thousands already watched), but Jody at Welding Tips and Tricks dot com has good things to say about 2% lanthanated tungsten. He also says typical filler for steel is er70s2, and 308L for stainless.

    http://www.weldingtipsandtricks.com/...ding-tips.html
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  6. Default

    thanks dave

  7. #7
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by DaveO View Post
    Jody at Welding Tips and Tricks dot com has good things to say about 2% lanthanated tungsten.
    Yep, I tried them all when I started and the lanthanated wound up my favorite, starts easy and stays sharp.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  8. #8

    Default

    I'd put some 3/32 2% lan (light blue) tungsten in and forget it. There are very few applications where changing the size will make much difference. If you are welding extremely think material at low current, just put a bit sharper point on it.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

Similar Threads

  1. tig noob in need of some help
    By steve1989 in forum General Welding Questions
    Replies: 10
    Last Post: 12-31-2013, 02:15 AM
  2. Noob in need of help
    By Chuck_jkl in forum Introduce Yourself
    Replies: 10
    Last Post: 01-24-2013, 02:17 AM
  3. noob
    By bubbas55 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 11-08-2012, 01:23 AM
  4. Noob to Tig
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 04-06-2011, 04:46 AM
  5. Noob from CT
    By Bikenstitchz in forum Introduce Yourself
    Replies: 3
    Last Post: 03-26-2011, 03:13 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •