Greets

Sorry for the newbie questions again but what do you think is causing this brown discoloration/dust? I have the 210 set up on DCEN and have tried low-high Ar (100%) gas flow. I have 3 sec of pre flow and 5 sec of post flow. The discoloration seems to track the angle of the TIG torch. i.e. the contamination is mostly in the direction of the gas flow. I was using a 3/32" 1.5% lanthanated electrode. Amps were set at 50. I did grind the metal but didn't wash it down with acetone. I'll get some acetone tomorrow.

The plasma looked OK/stable but I have zero experience with TIG welding so I can only compare to what I've seen on videos.

Attachment 10528

I'm SURE there are other issues with the set up but I thought I'd start with this funky contamination issue. Bad gas or bad setup/operator???

cheers
JohnG