Started to weld sum aluminum the other week and my machine seems to be stuck in pulse mode but it’s not on pulse. The arc cuts in and out I’ve messed with the balance frequency and doesn’t seem to change anything using the foot control or torch buttons same thing. It welds fine in dc pulse spot timer all work fine I haven’t been able to get in touch with support recently ray emailed me back once and left a message I called back and left a message also seems like it’s trying to ball the tungsten like the inverter is switching to negative but the positive side is cutting out in the cycle i really don’t know how else to explain it. I work in the power industry as a millwright/ power plant operator , I know my way around electronics pretty well for the most part and have a pretty good understanding how the inverter based welding machines work and I’m decent welding aluminum. Just wondering if anyone else has had any problems or where to start to look as far as troubleshooting thanks.