well its been a long time since i have really done any daily tig work 7yrs or so and that was on a 300 dynastyany how can someone get me in the pall park for settings on my 205?? i am trying to weld 14g sheetmetal i have it set at 70amps with foot pedal 2t on but want to try the pulse mode i think i have blue 2% 3/32 tungsten what i got with my 205. i have not got a chance to really use this thing since i got it other than the plasma and i like that a lot so far
thanx




any how can someone get me in the pall park for settings on my 205?? i am trying to weld 14g sheetmetal i have it set at 70amps with foot pedal 2t on but want to try the pulse mode i think i have blue 2% 3/32 tungsten what i got with my 205. i have not got a chance to really use this thing since i got it other than the plasma and i like that a lot so far 
Reply With Quote