Share
Results 1 to 11 of 11

Thread: intermit pilot arc with CT520

  1. Default intermit pilot arc with CT520

    Set up machine and turned it on. Connected plasma cutter. The first five minutes were good untill it started to sputter. I replaced the consumables, and the same thing happened. Pilot arc is intermittent when switch is depressed. When arc is on, bringing the torch to the material to cut, causes arc to actually blow out. Pilot arc is very intermittent and blows out when close to material. Plasma cutter overall, cannot be used. Please Help. thanks
    Last edited by cardoc; 03-26-2010 at 07:32 AM.

  2. #2

    Default

    The CT 520 is a Canadian version only, just so people aren't confused. First make sure your polarity is correct. DC- for the torch.

    The points in the pilot arc may need adjustment. Please call tech support to get the proper adjustment procedures for your machine.

  3. Default

    I am at the factory this Week but i will be back on monday. What pressure is the compressor set at and what psi are you running through the regulator. to high a settings can cause problems with the pilot arc being blown out
    cheers
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  4. #4

    Default

    Not sure if you got things worked out. Feel free to contact tech support for help if not, 7 days a week. The number is located at http://www.everlastgenerators.com/Technical-support.php
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. Default

    I have not heard back from Cardoc . It may be the pressure was to high and when the torch was brought close to the material the air pressure would flow back and extinquish the arc.
    We have had a couple of situations like this .
    Cheers
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  6. Default

    Quote Originally Posted by Titan winch View Post
    I have not heard back from Cardoc . It may be the pressure was to high and when the torch was brought close to the material the air pressure would flow back and extinquish the arc.
    We have had a couple of situations like this .
    Cheers
    Sorry, for not replying guys. Its been crazy at my shop. The torch works a little better between 20 - 30 PSI. The issue still remains though. If i move the torch across a 1/8" plate, really fast, it stays lit but does not cut all the way through. If I go slower it cuts through but sputters across and just punches a bunch of holes. I find it sputters the same at all pressures from very low pressure, 10 psi and at very high, 60 psi. I also have not yet adjusted or calibrated anything internally yet. thanks

  7. Default

    Can you give me a call preferably when you are at the unit so we can go through the steps and try to figure out what the cause might be.
    Thanks
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  8. Default

    Hey there, so my plasma torch really has not worked well ,at all, since i have bought it. I have to pull the trigger about 30 times before the pilot starts, then as soon as i get close to cutting the material, the arc stops and its just compressed air. Sometimes it starts if i hold the tip very close to the material, but that is rare when that happens. 99.9% of the time, the cutter will not arc with the first pull of the trigger. Is there a number that i can phone that is toll free? Getting really frustrated with the machine, thanks.

  9. #9
    Join Date
    Jul 2010
    Location
    Port Saint Lucie , Florida
    Posts
    85

    Default

    Cardoc,
    A few questions that I have that have not been asked and aslo I am not familiar with the 520 unit either. The air lines that you are using per your screen name is that you have a shop, so are you sure you are using dry air for 1 and also a lot of shops will use a in line oiler for a big system so is there an oiler in the system? I would assume not but just checking .
    Next thing is are you grounding or using the " work clamp" on your material? try not connecting the work clamp to see if that makes a difference. I had a 256 that I had the same type problems with a HF board and if I did not connect the work clamp it would cut great so give that a shot be careful to make sure with wearing gloves and do no have any bear skin leaning on the cutting metal or table when not using the work clamp on the materials.. I changed out the HF board and had no problems BUt like I had said earlier I do not know the 520 machine..
    Gary

  10. Default

    Quote Originally Posted by cardoc View Post
    Hey there, so my plasma torch really has not worked well ,at all, since i have bought it. I have to pull the trigger about 30 times before the pilot starts, then as soon as i get close to cutting the material, the arc stops and its just compressed air. Sometimes it starts if i hold the tip very close to the material, but that is rare when that happens. 99.9% of the time, the cutter will not arc with the first pull of the trigger. Is there a number that i can phone that is toll free? Getting really frustrated with the machine, thanks.
    Hi Cardoc, Duncan is currently at the factory and will be returning on the weekend, he has not been online to see your most recent post, you can give us a call at 905-630-8246 or send a pm with your number and we will give you a call ans see if we can get you unfrustrated. Jean
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  11. #11

    Default

    If you call our tech support line, we can call you back? Or call 877-755-9353. I posted a link back in March in this thread.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. No Pilot Arc with PP256
    By deepsnow in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 05-30-2014, 07:43 PM
  2. CT520 Plasma cutter consumables
    By cardoc in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 11-01-2012, 11:54 AM
  3. HF start or Pilot Arc
    By Odyknuck in forum Everlast Plasma Cutters (PAC)
    Replies: 12
    Last Post: 09-19-2012, 02:01 AM
  4. CT520 broke down
    By Martygras in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 04-22-2011, 09:43 PM
  5. NO HF arc start on my CT520
    By jonc in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 03-15-2009, 12:08 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •