Share
Results 1 to 2 of 2

Thread: arc force control for powertig 200lx

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default arc force control for powertig 200lx

    i have had a the powertig for almost a year and every thing works great with a water cooler and a flex head 225 amp watercooled torch and i have tried to get my stick welder to weld the best it can even tho it has no arc force and any help in making it make very good looking welds would be appreciated like for example should i stay on ac or dc and what rods should work the best since the power tig 200lx has a fixed setting for the stick welder and occassionaly i get fustrated haha

  2. #2

    Default

    The amperage is adjustable. But the arc force has more to do with helping out with cellulose electrodes. Stick welding takes a different skill set to master. I don't know but most people think that the lx does real well with most electrodes except the 6010 that is a cellulose rod.

    Typical excellent rods are 6013,7018, and 7014 or any iron powder rod should work well.

Similar Threads

  1. Powertig 185 Finger Amp control 17 Series torch availability
    By Benthos in forum TIG Welding (GTAW/GTAW-P)
    Replies: 45
    Last Post: 04-19-2014, 05:04 AM
  2. CK Rotary Amperage Control with Powertig 250ex
    By Cippee in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 01-07-2014, 05:12 AM
  3. 2012 Model Powertig 200dx control panel
    By bnun12 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 07-14-2012, 07:02 PM
  4. PowerTig 200LX Aluminum noob pics
    By Mad-Dax in forum Hobyist Projects
    Replies: 29
    Last Post: 04-15-2012, 09:26 PM
  5. PowerTig 200LX limited amps problem???
    By Mad-Dax in forum General Welder Questions
    Replies: 6
    Last Post: 09-11-2009, 02:57 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •