Hi fellas,

I've read a number of forums, and I am still at the starting point.

I just acquired an Everlast Power Pro 205. I am having trouble with the main amperage control. Apparently it is always starts at around 100 amps. That's with or without the foot pedal connected. After reading some posts, I'm pretty much ignoring the readout on this machine and going by what's happening to my puddle.

The way I can tell is the electrode is getting too hot and my puddle is way to large. No matter where i set the control, I get the same result.
Tried steel, stainless, and Aluminum(on AC with ~100Hz and 70%). My shielding gas(UHP-Argon) is at 20 cfh. Used 3/32 Thoriated with sharpened electrode(professionally sharpened) and No.7 cup. I also tried 1/16 electrode...same thing!

I am wondering if the rheostat (control knob) is bad?

Has anyone had a similar issue?

I'll be calling Mike at Everlast tomorrow(if open?).

Thanks,

Love this forum...lots of helpful info!