can some one give good directions on doing a fillet weld on steel. torh angles?
can some one give good directions on doing a fillet weld on steel. torh angles?
I try to stay vertical, not more that 10-15 degrees from there. Also, I like a short stick out normally 1/4" or less. Push the pool.
Mike R.