    Default Cooler Fluid

    In the process of setting up a 250 ex with cooler. What is the recommend fluid or mix? The pamphlet that came with the cooler does not indicate.

  2. Default

    Distilled or Deionized water. Do not use anti-freeze or tap water. Tap water will create mold and you run the risk of clogging the small lines on the torch. a lot of Anti-freeze is specially formulated to help seal small holes and that to could clog the lines. You could also by specially formulated tig coolants but they are a little more pricey.

  3. #3

    Default

    Dis weld,

    Sorry, I do not mean to flame you, but

    Miller makes a water cooler antifreeze and in general an RV type fluid is safe for our machines. It cost a little but definitely better than having a water cooler freeze in the winter or a torch freeze. Tap water is avoided if possible not because of mold but because of other deposits. Mold will form eventually even with distilled water.

    Regular antifreeze is not recommended, but with that said, there are thousands of water coolers out there with that in them.

  4. #4

    Default

    I have some shops here that just use RV & MARINE ANTIFREEZE in there machines and have not had any problems . that what i use in my machine cooling unit since they have not had any problems for years using it and its bidegradible and safe since is use for rv drinking water systems in motor homes in winter when not being used, it only like 4 buck a gallon from camper world . never use automotive coolant will plug your torch head . I us 1 gallon to 3 gallons of distiled water since it never get too cold here in the winter at Parker az , never use tap water eather .

  5. Default

    you do not mean to flame me.....What does that mean?
    RV coolant is conductive and will rob HF. Automotive anti-freeze is not only conductive but the additives in it will attack copper. Everything in a tig system is copper. If you do not have to worry about freezing temps just use distilled water, if you are to worry about freezing temps you should really use a low conductivity coolant, just make sure it it designed for Tig.
    Last edited by DisWeld; 04-01-2010 at 01:09 PM.

  6. #6

    Default

    RV fluid is fine. It is used widely. Its formulation is very similar to some of the water cooler coolants on the market and that is why its used. Our products are safe for use with it. The construction of our coolers are fine.

    Rob HF? Sure a lot of things rob HF. Its a theoretical situation... It really is only a very small amount compared to what ours generate. But our units only use HF to start and NO problems with starting have ever been reported with it.

  7. #7

    Default We're cool now

    Thank you all for your help. And, yes, my issue is where the equipment is stored when not in use - below freeze several months a year.

  8. #8

    Default

    A gallon or two of the "real" water cooling fluid is not too expensive when you compare it to the cost of a new cooler. Last I checked it was about 20.00 here.

  9. #9

    Default coolant information

    FYI
    You might find this interesting. Not definitive, just more information.
    http://newsgroups.derkeiler.com/Arch.../msg00161.html

  10. #10
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Default

    This subject is of particular interest to me, being in Alaska. Dose anyone have an idea what the “real” fluid is made of? Has anyone anywhere tried alcohol? I know its flammable but a 40% mix will not light and won’t freeze to about -40 F. There is some air dryer fluid (for truck brake systems) that’s less flammable also but I think it also has some kind of glycol in it. You can get a gallon of denatured alcohol at Wally World for about $7 in the paint dept.
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

  11. #11

    Default coolant mix

    If you look up the MSDS for Miller's coolant, the only listed item is glycol.

  12. #12
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Default

    Thanks, that’s a clue, I noticed the guy doing the testing (the link you posted) didn't test the Miller fluid? I'm probably going with the RV fluid, my original plan, and maybe change it often. I suppose though that Mark has a good point, cost of the "blue" fluid far outweighs replacing the cooler or mucking up the torch. And hey we already saved big bucks on the setup anyway, right.
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

  13. Default

    Quote Originally Posted by dlong View Post
    In the process of setting up a 250 ex with cooler. What is the recommend fluid or mix? The pamphlet that came with the cooler does not indicate.
    I have read this thread about coolant and gone to the Miller site and many others trying to figure things out. What's so special to charge $25 per gallon for TIG/MIG coolant with HF start. It was as I suspected, Miller doesn't make the coolant but a distributor in Florida called Star Brite. They make a variety of products related to automotive and recreational market.

    http://www.millerwelds.com/pdf/msds/Coolant043810.pdf
    http://www.starbrite.com/

    So from my reading it is EG(ethylene glycol) mixed with deionized water(distilled water works too) probably in a 50/50 mix.

    http://en.wikipedia.org/wiki/Ethylene_glycol
    http://en.wikipedia.org/wiki/Deionized_water

    So can anyone tell me why just regular EG from the auto parts store, maybe the cheaper stuff with no other additives wouldn't work? And not have to pay the high prices others want to charge plus shipping?

    UPDATE

    Okay, I went to the auto parts store and looked at the selection and thankfully the contents are listed for the most part. There were ones that stated it worked for Aluminum I knew would not work. I found some with additional additives for corrosion protection. I settled on PEAK Long Life which list the contents as Ethylene Glycol (107-21-1), Diethylene Glycol (111-46-6) and Water (7732-18-5). So this looks to be identical to the Miller/StarBrite stuff for less than $15 for 2 gallons. I will do a a 50/50 mix and see what happens
    Last edited by Intrepid; 08-14-2010 at 04:33 PM. Reason: Update

  14. #14

    Default

    Myself I just use distilled water, but what about windshield washer fluid? why wouldnt that work?

  15. Default

    Guy's ...... there are only two things that really matter. One, is it corrosive? and two, does it contain coagulants like those in some automotive coolants. Otherwise have at it and report back! You could probably use Alpaca urine, .... i dunno. Tap water, hose water, etc, are eventually going to calcify, and lime up your little torch pathways. But i guess thats why they make CLR, and lime away. Some auto coolants have radiator coagulants to help guard against small leaks. RV coolant is a different formula. Distilled water, .... sure why not. As far as sub zero temps, .... god bless ya if you can weld in that enviroment! lol! If just occassional work, just dump the water when your done, what is it, ... 2 gallons of distilled?

    Don't get me wrong here my friends, just bein a little tongue in cheek to lighten it up! There's lots of ways to skin a cat!
    Last edited by trackmaster; 08-09-2010 at 06:08 AM.

  16. #16

    Default Using "pink" fluid

    I have been using pink RV anti-freeze(propylene glycol based) fluid in my home made cooler set-up with a PP256 and it starts/welds perfectly. I even added 6oz of "radiator anti-rust with water pump lube" to the mix when I noticed my pump, an in-tank automotive fuel pump, getting rusty. By using a submerged 12v.DC pump and all the various fluids of the mix, I'm probably breaking lots of rules, but this has worked fine since I got the welder in June. I will post any problems that might arise.

  17. #17

    Default Pink RV fluid use update

    Just checked the pump in my cooler set-up. Still no rust, pressure(30psi) and flow (1 qt/min.) are fine, but there patches or green mold floating on top of the coolant in the tank. Probably not a good thing.

Similar Threads

  1. Cold Weather Power Equipment Starting Fluid on Steroids: Propane!
    By fyidiy in forum Personal Projects (no welder required)
    Replies: 0
    Last Post: 09-03-2018, 04:26 PM
  2. tig cooler
    By postmark in forum Welding Projects and Pictures
    Replies: 1
    Last Post: 01-07-2015, 12:26 AM
  3. Tig cooler cooler power source - "warning"
    By Odyknuck in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 12-17-2012, 09:37 PM
  4. Cooler
    By dave s in forum Pre-sales, Sales and Shipping questions
    Replies: 0
    Last Post: 12-12-2011, 01:49 AM
  5. Anyone get a new Cooler Yet?
    By Zoomie in forum General Welder Questions
    Replies: 15
    Last Post: 06-25-2011, 03:29 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •