  1. Default Argon Tank Empty?

    I am a hobbyist and been working on getting better at TIG welding aluminum.

    With that, I bought a full tank of Argon a couple of weeks back and set the flow to about 15 cfm and it read 2000 psi full. It reads 1000 psi now.

    The arc sputters and jumps even at high frequency AC like it is contaminated. Could I be out of Argon even though it reads 1000 psi?

    Thanks in advance for any feedback.

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Buggy Chief View Post
    I am a hobbyist and been working on getting better at TIG welding aluminum.

    With that, I bought a full tank of Argon a couple of weeks back and set the flow to about 15 cfm and it read 2000 psi full. It reads 1000 psi now.

    The arc sputters and jumps even at high frequency AC like it is contaminated. Could I be out of Argon even though it reads 1000 psi?

    Thanks in advance for any feedback.
    Not empty until you hit the regulated pressure. (Usually 40-80 psi) But you could have a leak somewhere that is sucking in air. Also there is the possibility of a bad bottle of gas. Were things OK when you first got the bottle? Is your material really really clean?
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    Nevermind...Pressure doesn't tell the story. It's weight. I have a 80 bottle and it should weigh about 60 lbs full and it is weighing about 50 now, which means empty. Empty bottle weight is 50ish.

    Answered my own question.

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Buggy Chief View Post
    Nevermind...Pressure doesn't tell the story. It's weight. I have a 80 bottle and it should weigh about 60 lbs full and it is weighing about 50 now, which means empty. Empty bottle weight is 50ish.

    Answered my own question.
    There is a lot of weight variation between bottles, especailly the smaller ones. Unless you have the exact tare weight for that bottle, you can't go by weight. Besides there is no way an empty argon bottle will have 1000 psi. It is a compressed gas not a liquid like CO2.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Argon Tank price?
    By Elantramax1 in forum General Welder Questions
    Replies: 38
    Last Post: 02-05-2015, 11:18 PM
  2. Just upgraded to a 250 CFT argon tank.
    By Steve in forum TIG Welding (GTAW/GTAW-P)
    Replies: 33
    Last Post: 11-17-2013, 12:23 PM
  3. Ballpark idea of argon tank time...
    By Ray C in forum General Welder Questions
    Replies: 3
    Last Post: 08-08-2012, 10:19 PM
  4. How empty is empty
    By Ron66 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 05-31-2012, 03:25 AM
  5. ARGON and ARGON/CO2 TANK SIZES
    By everlastsupport in forum Technical Bulletins and Tips
    Replies: 47
    Last Post: 10-13-2011, 05:19 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •