    hey all, has any one that owns a everlast power tig 200 dx ever used it in stick mode? ive done tons of stick welding on other machines but oddly when i tried this unit for stick the electrodes would turn orange while welding :S Can any one shed some light on why this would happen? using 1/8 7018 on dc positive

  2. #2

    Default

    Quote Originally Posted by steve1989 View Post
    hey all, has any one that owns a everlast power tig 200 dx ever used it in stick mode? ive done tons of stick welding on other machines but oddly when i tried this unit for stick the electrodes would turn orange while welding :S Can any one shed some light on why this would happen? using 1/8 7018 on dc positive
    No reason to look at the machine,,,,more likely the rods are contaminated...7018 rods can suck up moisture really fast...the change of color is probably due to sweating out...as you use them..
    Some of those lies people tell about me, are true

  3. #3

    Default

    I have used mine stick welding with a lot of different rods, Some rods require oven storage and some do not !, your situation is a common one that i have seen for years moisture from humidity or another source.
    I had an employee that was running some 7018 rods that evidently had some solvent or oil on them . The flux was nasty green colored and the weld poor.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

Similar Threads

  1. 250ex arc problems welding on ac but not dc ?????
    By slufoot2005 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 10-12-2013, 02:48 PM
  2. Stick welding aluminum?
    By undercut in forum General Welder Questions
    Replies: 14
    Last Post: 05-13-2012, 11:48 AM
  3. Preheating to help Stick Welding
    By undercut in forum Stick Welding (SMAW)
    Replies: 5
    Last Post: 05-07-2012, 07:30 PM
  4. low amperage stick welding with PU 205
    By worntorn in forum Stick Welding (SMAW)
    Replies: 2
    Last Post: 05-03-2011, 12:21 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •