Originally Posted by
performance
Two points worth noting, as context is important.
1) This is a limited release of the new 210ext unit, as we prepare for full production. It's very different in many respects than the current unit and has more/different capabilities than the current unit including a higher duty cycle, larger case, different factory etc.
2) Paul's unit, last I knew was a 225lx unit (and not a digital 210ext) which is analog and all analog units use the 2T function in conjunction with the pedal as it is the same circuit. Slope works on this unit, but there are NO start amps or end amps, and it always starts at the lowest capable amperage, and ramps up from there. The upslope and downslope must be turned down or off to run the pedal normally or operational issues will occur.