I am looking at buying one but I want to know what you think of yours and how do you use it. I have a few concerns about it. First I see that it goes up to 26 volts. I weld pretty heavy metal and am wondering if it will go into spray transfer with .035 wire. I have a millermatic 200 . It will go up to 260 amps at 35% duty cycle and it will go up to 30 volts. To go into spray transfer I have to run it at 28 - 30 volts. At 26 it is still in short arc but is on the edge. If I lowered the wire speed a little I might get into spray . Then can you get a 15 foot gun with it or what after market mig guns will fit it. The next thing would be how do you like the way it stick welds. Does it do ok with 6010 rod and 7018? I do not know if I will use all the bells and whistles that the machine has but I need the capacity and portability. I have been dragging my 200 around but it is so big that it is a hassle that I would rather do without. I sure wish it would go up to 28 volts though.