I pu costing me time archased the supercut 50p it work for about about an hour. I cut a a total of maybe 12 inches of 1/4 inch thick material. And the machine died. I sent it back and waited for 5 days and the new one lasted 3 days and it start sparking and not cutting. Now the alarm light is on and it will only blow air. Has anyone had this problem or know how to fix it. This is extremely aggravating and it's costing me lots of time and money. Just to be clear I'm running it on 220 which I have checked. Everything is hooked up correctly. I have put all new consumables in it. It's clean metal grounded good. I have many filters on my air system.