PP205 problems--
I use only the TIG about once every 3 months. Yesterday it turned into scratch start only without gas control unless you turn the machine (or bottle) off. The amp figure never gets above 36.
The OEM torch set on 2T starts gas, but power is already present.
It sounds like it lost its mind?