Thread: 200 DX - Pulse question on AC

Hybrid View

bmeyer6472 200 DX - Pulse question on AC 09-14-2014, 10:56 PM
performance Yes. 20 amps is the bottom. ... 09-15-2014, 02:28 AM
bmeyer6472 Thanks Mark - that's what I... 09-15-2014, 02:40 AM
Previous Post Previous Post   Next Post Next Post
  1. Default 200 DX - Pulse question on AC

    The 200 DX is rated down to 20 amps in AC mode. Does this restrict the pulse amps to no less than 20 amps also?

  2. #2

    Default

    Yes. 20 amps is the bottom. Think about it, If it was one amp that was the minimum, how would you expect pulse to work? Practically, the reason the unit is limited to 20 amps is that is bottom end that the unit can hold a stable arc. We have the 250EX, 210EXT, 255EXT etc, that can start and hold an arc at much lower amps in AC, but they are also more expensive. But even if it is 5 amps....you will bottom out the capabilities of the pulse the closer you go to the minimum amperage. For example, if you set it for 5% pulse amps, and the unit is set at 30 amps...you will 20 amps as the bottom or the unit will cut out the arc.

  3. Default

    Thanks Mark - that's what I thought, and it makes sense. But I can probably live with 20 amps anyway! :-)

Similar Threads

  1. 200DX/pulse question
    By chrispy350 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 02-22-2015, 01:47 PM
  2. New Everlast Pulse on Pulse Machines?
    By m10za in forum Pre-sales, Sales and Shipping questions
    Replies: 3
    Last Post: 02-04-2015, 07:53 PM
  3. WHo uses Pulse on DC?
    By Johnson in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 03-11-2013, 09:17 PM
  4. Question re: operation of pulse mode on PowerTig 200DX
    By Tantalum711 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 07-08-2011, 10:21 PM
  5. Power Tig 225LX Pulse Question
    By MikeGyver in forum TIG Welding (GTAW/GTAW-P)
    Replies: 25
    Last Post: 06-15-2011, 01:47 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •