Quote Originally Posted by Winky View Post
OK I'll admit it ... I go to HF sometimes but am always very careful about what I buy ... I'm really not impressed with their consumables ... however I have used their flux core ... eh ... not terribly disappointed with it.
Winky, Where the heck you been.

Yea, I have bought HF wire and Home Depot Lincoln wire and never had a problem. HF is what it is, you try things, some good and some you swear off. No drill bits or sand paper for sure. I figure a lot of times it's a one time tool. I have had a orange grinder for almost 10 years. But the price and the 25% off that. Who can resist.