225LX problems
I'm getting excessive arc that's seems like it's maxing out the machine and melting everything in it's path.
This happens with my cheap Harbor Freight inverter TIG but it shouldn't be happening with the 225.
Right now I'm trying to tack some twisted MIG wire on a belt-buckle. I'm using 2T @ 85 amps on the torch button and momentarily touching the button. About one out of ten tried I get a good arc. Half the times it buzzes like the ground isn't attached or it blows the wire completely off the belt buckle. I've had to cut and re-weld a half dozen times already.
![](http://i105.photobucket.com/albums/m208/jtybt/Things/004-2.jpg)
What is causing the problem?
Charlie
Everlast 225 LX
Everlast PP 50
HF 130 TIG/90 ARC
HF 90 fluxcore
ATX MIG (don't ask)