    Hello guys, I'm new to the forum but I've had a 200DX since about March of last year. Yesterday I was welding on some aluminum and the machine quit welding. I had a current alarm on the front panel. There is still a minimal arc but not usable. I called tech support and explained what happened and was told that I will have to send it in for repair. I asked about the turn around and he said right now they are looking at 6 to 8 weeks. Not to mention I have to pay shipping both ways. My question is, has anyone had this happen and is there anything I can check prior to sending my unit in for repair.

  2. #2

    Default

    You could talk with Mike. (PM him first at everlast support). He's pretty good at on the phone diagnosis and if possible repair rather than sending it in. Of course, it is very likely that you will if that is indeed the issue. If you have the skills it is possible to make some repairs.

  3. Default

    Thanks Mark. I will give that a try.

  4. #4

    Default

    Sammy just be sure not to do anything that will void your warranty.
    and welcome to the forum.
    Lincoln A/C 225
    Everlast P/A 200

  5. Default

    Thanks but now I have to show my ignorance. I haven't been active on many forums and not sure how to go about PMing. Mark advised I should PM Mike but how do I find him to send a PM?

  6. #6
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Here's one way: in the upper right corner of your screen, click the Notifications link. A little window opens; then click Inbox. That gets you to your inbox, where you can click the link for Send New Message, along the left border of your screen. In the Recipient box start typing in Mike's screen name, EverlastSupport.

    Good luck with it, I hope it's something you can fix on the phone with Mike.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  7. Default

    Thank you very much Dave. I was able to get the PM to him with your help.

Similar Threads

  1. Current Requirements for Plasma's
    By sportbike in forum Everlast Plasma Cutters (PAC)
    Replies: 12
    Last Post: 07-02-2012, 08:05 AM
  2. 256 a bit of trouble
    By ducksface in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 16
    Last Post: 05-20-2011, 08:03 AM
  3. PM 256 2T/4T trouble
    By dwdw in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 04-03-2011, 06:14 PM
  4. Supercut 50 over current light
    By outsidegangskilled in forum Everlast Plasma Cutters (PAC)
    Replies: 2
    Last Post: 09-11-2010, 02:25 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •