  1. Default PP164 cutter trouble?

    Several times today trying to cut some angle my PP164 would only fire the starter arc but no cutting arc.
    Then if the cutting arc did start, while in the middle of cutting, the arc would simply quit as though I had released the trigger, then spontaneously start again....all while continuously holding the trigger.
    I finally got the cut made but it was a mess.
    Any ideas?
    Is this a symptom of misadjusted points?
    Ground was attached directly to the part being cut, and the green light was on saying OK to cut.
    Thanks, John
    שלום

  2. #2

    Default

    The unit does not have HF starting, so the HF points do not work for this. I'd check for worn consumables, missing swirl ring, or loose consumables. Also verify air pressure and dry air. OK to cut does not mean it is ideal to cut. You may need to raise your pressure.

  3. Default

    Thanks Mark, I'll check those things...one thing I didn't mention was that I installed one of those $8 harbor freight dryers.
    Maybe that was messing with my air flow.
    שלום

Similar Threads

  1. PP164 Flow meter
    By JohnT in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 04-10-2018, 03:22 PM
  2. Amazon 210EXT Price at $1649 and PP164 at $1299, Free Shipping Too!
    By christian in forum General Welder Questions
    Replies: 0
    Last Post: 11-25-2015, 05:45 PM
  3. Pp164
    By klavalley in forum Pre-sales, Sales and Shipping questions
    Replies: 6
    Last Post: 07-10-2013, 03:38 PM
  4. 256 a bit of trouble
    By ducksface in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 16
    Last Post: 05-20-2011, 07:03 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •