    Has anyone had water mixed in with their argon? The cup appears to be wet after trying to weld a bit.
    Everlast 250EX
    Lincoln Powermig 255
    Firepower 130

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    It happens more than you know. We have not had a complaint for a bit. But it does happen. Take is back and see if they will exchange it for you.