need opinions on flow rates as LPM vs CFH .Are all Everlast regs calibrated LPM?
I am Welding .250 wall 2x2 square steel tubing.
need opinions on flow rates as LPM vs CFH .Are all Everlast regs calibrated LPM?
I am Welding .250 wall 2x2 square steel tubing.
Yes all our regulators are currently in lpm. Multiply by 2.1 to get cfh.
Doug it depends upon whether its mig or tig and the conditions...but for tig about 7 lpm or 15 cfh and for Mig 10-12 lpm or 20-25 cfh.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
Check here for a quick conversion list
http://www.everlastgenerators.com/fo...read.php?t=261
Make sure you have no air movement as well (fans in the shop, welding outside).
Mike R.
Email: admineverlast@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x203
M-F 12 - 7PM PST
FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.