 Originally Posted by 
chrispy350
					
				 
				Love the 200DX Tig welder.
Is it just me, or does it seem that as you come off the pedal mid-weld, you lose the effectiveness of the pulse?
I'm using a very slow tempo, on the order of 1-1.5pps on some thin aluminum (1/16) and as I'm working my way across and want less heat and roll off the throttle, I just get a steady arc, rather than the hard 'on/off' I had previously.  Should the pulse be functional regardless of the pedal position?
Thanks in advance--
Chris
			
		 
	 
 Perhaps the pulse amps percentage is the percentage of the panel setting, not what the pedal is set for. So as you lower the output you could fall under that setting and lose pulse. Just a guess, but I know on machines that have a pulse amps instead of pulse percentage, that is what happens. If you are only welding at mid pedal, I can see that being more likely. Try adjusting your max amps so that you can do most of the weld at full pedal, then just back off a little as things heat up. It may be a combination of design and parameters. I'm sure someone from Everlast can supply the details about their pulser design and settings for that machine. Also when you have an issue, it is always helpful to post all your settings.
				
			 
			
		 
			
				
			
			
				Long arc, short arc, heliarc and in-the-dark!