  1. Default Guide for PU205 Plasma Torch?

    I'm curious if anyone knows if there's a circle cutting / straight edge guide available for the AG60 torch that comes with the PowerUltra 205 or if any of the kits available for other brands (Miller, Hypertherm, etc) will work? I assume it's purely based on diameter of the cup on the torch, but that may be a bad assumption or if it's not I don't know the diameters of other torches to know if they match the PU205 AG60 Torch.

    I'm looking for something along the lines of these examples:
    http://www.pipefitter.com/existing_php/Plascut.php

    http://www.weldfabulous.com/Plasma-C...40969-3-1.html

    http://www.thewelderswarehouse.com/W...Guide_Kit.html

    Thanks
    Ralph

  2. #2

    Default

    Do not recall the brand, but there is one company that sells them in three sizes (diameters). They have set/lock down screws to attach them. If I find the name I will post it here for you.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #3

    Default

    A lot of these units use a locking collar or something similar to hold the torch head. I believe you could get a locking collar that would fit the outside diameter of the torch head and adapt it to about any style.

    Then if you are welding, you might as well make one. They are fairly easy to make. I'll try to put one together in the next few weeks out of common parts. I'll get a little tool steel stock and try to make something.

  4. #4
    Join Date
    May 2010
    Location
    West Seattle
    Posts
    23

    Default

    I've made 1 before for my old Mitech 120. A word of warning, use the largest magnet you think you'll need or go up 1 size. I did 1 similar to the thermal dynamic with 2 bars. It worked great as a circle cutting jig if you held the magnet down.

    Cliff
    A warped mind is a wonderful thing to abuse

Similar Threads

  1. Think this is cool plasma guide and copy
    By Rodsmachineshop in forum Everlast Plasma Cutters (PAC)
    Replies: 6
    Last Post: 04-24-2012, 04:37 PM
  2. Plasma Roller Guide?
    By Buggy Chief in forum Everlast Plasma Cutters (PAC)
    Replies: 10
    Last Post: 04-01-2012, 11:10 PM
  3. Plasma Cutter Guide
    By SeanMurphy265 in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 04-26-2011, 12:38 AM
  4. Power Ultra 205 Plasma Ceramic Tip with guide ridge?
    By ralphhood3 in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 05-20-2010, 10:49 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •