Hi all. I have a Hobart Auto Darkening helmet. Its been doing something weird lately. When I am welding, Sometimes it goes so dark you can barely see the Arc. Other times, I am done welding, The lenses stays dark. Until I press the Reset button. This is a good minute or so after I am done. Delay is not set long. Whatever the default arrow is pointing to. Had to turn the shade to #9. Was on #10. Sometimes it flashes. The low battery light has not come on. I am wondering if I should contact Hobart and see about a Warranty repair. But I need it for work.