    Default PowerTIG 185 questions.

    On my older model 200DX, if I plugged in the foot pedal, I didn't have a way to set the amperage at let's say 100 amps. If the pedal was plugged in, it would go all the way to 0-200. And I couldn't set the amps at a certain amperage, and the amps wouldn't go past that.

    On the PowerTIG 185, is it the same way? Or can I set the amps, and with the pedal pressed all the way down, it won't go past it?

    Thanks
    Purple Fabricator 211i

  2. #2

    Default

    Did you get my email? To sum up: The 185 and the 200DV(DX) maximum amps are set on the panel.

  3. #3

    Default

    I did thanks. Just wanted to make sure before I picked one up.
    Purple Fabricator 211i

Similar Threads

  1. PowerTig 250EX questions ---- foot pedal
    By 11Bravo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 09-07-2018, 02:53 AM
  2. Questions About I-Mig 140
    By esg612 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 16
    Last Post: 02-22-2017, 06:26 PM
  3. PowerTig 185 questions
    By sportbike in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 04-19-2013, 07:19 AM
  4. 256 questions
    By tnc110 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 43
    Last Post: 05-02-2012, 01:03 PM
  5. Pu 205 questions please
    By Dne007 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 03-13-2012, 08:12 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •