Posted on WeldingWeb over the weekend but got no responses so I figured I'd post here and see if someone could help me out...
I'm looking for some extra ceramic tips (collars?) for my PowerUltra 205 60amp Plasma Torch. Only problem is what it came with and what shows as the consumables on the everlast site appear to be different.
What it came with was the taller cone with the rib in the middle for mounting the wire standoff guide, and the end of it sticks about halfway to the end of the nozzle like what's in this picture:
http://www.everlastgenerators.com/pr...ails/318_7.jpg
The consumables on the site (and what's available other places) all seem to be the shorter cone without the ridge for the wire standoff guide and don't cover nearly any of the nozzle like this:
http://www.everlastgenerators.com/pr...ails/592_1.jpg
I got some of the 2nd ones, and while they're supposed to work on my torch they don't screw on. The thickness of the base of the ceramic tip is a hair too thick, and as a result it won't go over the slight ridge at the base of the head of the torch.
So a) I'm looking for the ceramic tip that I can use with the wire standoff guide, and b) I'm looking for something that'll fit
Anybody know where to get the longer ceramic tip with the ridge for the guide, either from Everlast directly or through somewhere else (eBay?)
Thanks
Ralph